Foundations on permafrost — how to dimension CemPU construction

Permafrost is not a static layer — it reacts to the building's heat load, surrounding climate change and water conditions. An incorrectly dimensioned foundation can thaw the soil under the building and cause differential settling of 100–300 mm. Here is how we dimension CemPU construction for permafrost.

In a nutshell

  • Point foundations or piles: Standard solution in permafrost areas — transfers building load below the active layer to stable frozen subsoil
  • Thermal bridges must be avoided: Direct contact between building and ground causes heat flow that thaws the permafrost
  • Thermal insulation on grade: 200–400 mm EPS under the building limits heat flow into the ground
  • CemPU's low point load: 60 kg/m² sandwich panel vs. 180–220 kg/m² for sand-lime brick — markedly lower foundation load
  • Geotechnical assessment required: Every permafrost site must be investigated individually — active layer depth varies 0.5–3 m

What is permafrost and where is it found in Greenland?

Permafrost is soil that has been below 0 °C for at least two consecutive years. In Greenland, continuous permafrost (depth >100 m) covers most of the country away from the coast, while coastal areas often have discontinuous or sporadic permafrost. The uppermost layer — the active layer — thaws each year in July–September and refreezes in October–May. Active layer depth varies from 0.5 m in the north to 3 m in the south and coastal areas.

What types of foundation are used on permafrost?

Four primary foundation types are used for permafrost construction:
1. Pile foundations: Steel or concrete piles driven down to stable permafrost below the active layer. Most used for larger buildings and institutions.
2. Point foundations on frost-free layer: Standard for single-family houses — foundations extended below the active layer to frost-free level.
3. Open-air pad: Building raised above the ground on concrete posts or piles with ventilated crawl space — heat flow into the ground is minimised.
4. Thermal pad: Thick EPS or XPS insulation under the building that limits heat flow to the ground — used primarily on discontinuous permafrost.

Why must thermal bridges between building and ground be avoided?

Heat flow from a heated building down into the ground is critical in permafrost areas. If the active layer under the building thaws over several seasons, differential settling develops — some parts of the foundation sink more than others. For a 150 m² house, the difference can become 100–300 mm over 5–10 years if thermal bridges are not handled correctly. This causes facade cracks, doors that bind, and in the worst case structural damage. CemPU's continuous PU core without mechanical breaks reduces thermal bridges in the envelope itself, but correct dimensioning is still required at the foundation interface.

What is CemPU's weight advantage for permafrost foundations?

CemPU sandwich panels weigh approximately 60 kg/m² — markedly less than traditional alternatives:
- Aerated concrete: 100–140 kg/m²
- Sand-lime brick: 180–220 kg/m²
- In-situ cast concrete: 250–500 kg/m²
- Timber frame: 30–50 kg/m² (but with fire weaknesses)
The lower point load delivers four advantages: 1) Fewer or thinner piles required, 2) Lower capillary lift risk if the active layer thaws, 3) Faster installation as crane capacity is not limiting, 4) Lower freight cost per square metre of wall.

How is CemPU adapted to permafrost projects?

Tekment delivers project-specific CemPU panels that include:
1. Reinforced bottom edge: Dimensioned to the actual pile loads and spans.
2. Thermal-bridge-free interface: Our standard detail with thermal break between foundation and the panel's bottom profile.
3. Ventilated crawl space solution: CemPU panels can be combined with ventilated post foundations, where the air under the building limits heat flow.
4. Thermal pad: 200–400 mm EPS directly under the panel's bottom edge for projects with discontinuous permafrost.
We work with geotechnical consultants in Greenland (typically MT Højgaard Grønland or Permagreen) on individual project dimensioning.

Frequently asked questions

What is permafrost?

Permafrost is soil that has been below 0 °C for at least two consecutive years. In Greenland, continuous permafrost (depth over 100 m) covers most of the country.

What foundation does permafrost construction require?

Point foundations or piles to stable frozen layer, combined with thermal insulation and possibly ventilated crawl space. Each site requires individual geotechnical assessment.

Can CemPU be used on permafrost?

Yes. CemPU's low self-weight (60 kg/m²) reduces foundation load, and panels can be combined with both pile foundations and thermal pads. Tekment dimensions to the project.

What happens if thermal bridges are not handled?

The active layer under the building can thaw over several seasons and cause differential settling of 100–300 mm — with cracks, binding doors and structural damage as a consequence.

How deep is the active layer in Greenland?

0.5–3 m depending on latitude and soil type. Coastal areas with water-rich sand/gravel soils have deeper active layers than mountain areas further from the coast.